logo

Standards Manage Your Business

We Manage Your Standards

SAE

SAE AMS5671H : 2019

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable

Standard Details

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars up to 4.00 inches (101.6 mm) exclusive in nominal diameter or thickness, forgings 4.00 inches (101.6 mm) exclusive in nominal thickness, flash welded rings up to 4.00 inches (101.6 mm) exclusive in nominal radial thickness, and stock of any size for forging or flash welded rings (see 8.6 ).

Cross Reference: AMS2261,AMS2269,AMS2371,AMS2374,AMS2750,AMS2806,AMS2808,AMS7490,ASTME10,ASTME354,ASTME8

General Information

Status : Historical
Standard Type: Main
Document No: SAE AMS5671H : 2019
Document Year: 2019
Pages: 9

Life Cycle

Currently Viewing

Historical
SAE AMS5671H : 2019
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +